Skip to content
Request a Quote
Menu
Placeholder for a photo (BH-A16-S01-I01)

Die Casting Design Guide

Design a die casting around how molten metal fills and leaves a steel die: thin, even walls with generous radii, draft on every face that slides against the die, and features the die can form with few moving parts.

Then decide which features will be machined after casting and which surfaces must stay free of porosity or marks. These choices are easiest to change in the model. Once the die is built, adding draft or moving a core means die work, another trial and new samples. The guidance below gives general starting points for aluminum and zinc alloy die castings. Suitable values depend on the alloy, part and die, so confirm them with your supplier before tooling.

Wall Thickness

Start with wall thickness, which controls filling, cooling and where porosity forms.

Keep Walls Thin, Even and Smoothly Joined

Metal enters a die casting die at high speed and starts to solidify as soon as it touches the steel. Thin, even walls fill and cool consistently. Thick sections cool last and can shrink into internal voids, known as shrinkage porosity, or sink at the surface, while adding cycle time and metal to every part.

Choose the thinnest wall that meets the part's strength and stiffness needs, and hold it as consistently as you can. Zinc alloys generally fill thinner sections than aluminum alloys, but the workable range depends on part size, flow distance and alloy, so take it from your supplier.

  • Make changes in wall thickness gradual rather than stepped.
  • Core out thick bosses, pads and solid areas.
  • Radius inside and outside corners, since sharp corners disturb flow, concentrate stress and wear the die.
  • Add ribs for stiffness instead of thickening the wall.
Placeholder for a diagram (BH-A16-S02-I01)

Draft

Even walls help the metal fill the die. Draft decides whether the casting then releases cleanly.

Add Draft to Faces That Release from the Die

Draft is a slight taper on faces parallel to the direction in which the die opens and cores withdraw. Without it, the casting, which shrinks onto cores as it cools, drags against the steel on ejection and can be marked or distorted.

Inside walls and cores

Inner walls and cores usually need more draft than outside walls. Check deep pockets and tall cores in particular, where the grip is greatest.

Aluminum and zinc

Zinc alloys can often be cast with less draft than aluminum. For aluminum, around one degree on outside walls is a common starting point, with more on inside walls. The right figure also depends on feature depth, so agree it with your supplier.

Faces that must stay straight

Mark faces that must be parallel for fit or sealing. They can be machined straight after casting, or the parting line can sometimes be placed so they need less draft.

Ribs and Bosses

Ribs, bosses and cores need draft too, and they are where even walls most often thicken.

Ribs, Bosses and Cores

Ribs, bosses and cored holes let a casting carry loads and fasteners without thick sections. Give each one draft and radii, and keep it in the die-opening direction where you can.

Ribs

Ribs add stiffness and can help metal reach distant areas of the part. Size them in proportion to the wall they join, with a radius at the base, and prefer several moderate ribs to one tall one.

Bosses

Core bosses out so their walls stay close to the nominal wall, and tie them to nearby walls with ribs. Threads are usually tapped or machined after casting.

Cored holes

Fixed cores in the die-opening direction form holes and pockets most simply. Slender cores can bend or overheat, so small, deep holes are often cast as a short pilot and drilled.

Side cores

Features at an angle to the die opening need a moving slide. Each slide adds die cost, maintenance and sometimes cycle time, so ask whether a design change could avoid it.

Placeholder for a diagram (BH-A16-S04-I01)

Porosity

Thick junctions are also where porosity forms, so decide next where it would matter.

Plan for Porosity and Critical Surfaces

Most conventional die castings contain some porosity. Gas porosity comes from air and lubricant vapor trapped as the metal fills the die at speed; shrinkage porosity forms in thick sections that solidify last. Design and process choices cannot remove it entirely, but they can keep it away from surfaces where it would cause trouble.

The surface layer, which cools first against the die, is usually denser than the core. Machining cuts through it and can expose pores, so plan these surfaces with your supplier:

Machined surfaces

Keep machining shallow on faces that must be free of visible pores, and keep those faces away from thick sections.

Sealing features

State the medium, pressure and allowable leakage, how sealing will be checked, for example by a leak test, and whether impregnation to seal porosity is acceptable.

Cosmetic surfaces

Mark faces where gate, overflow or ejector marks, flash or blisters after coating would not be accepted, before the die layout is fixed.

Conventional die castings are also generally unsuitable for welding or full heat treatment, because trapped gas can expand and blister the surface. Raise either requirement before the process and alloy are chosen.

Placeholder for a diagram (BH-A16-S05-I01)

Machining Allowance

Many of those surfaces are machined after casting, and the casting has to be designed for that machining.

Machining Allowance and Datums for Secondary Machining

Decide which features will be machined after casting before the die is designed, because the casting must carry extra metal there and offer reliable surfaces to locate from. Typical candidates are bores, bearing seats, sealing and mating faces, threads and features with tolerances tighter than casting can hold.

Machining allowance

Enough stock to clean up casting variation, draft and parting line shift, but no more, so the cut stays near the dense surface layer. Agree the amount for each feature with your supplier.

Casting datums

Stable as-cast features formed in one die half, away from the parting line, slides and ejector marks. Datum targets, a few defined points or pads, let the first operation locate every casting the same way.

Machined datums

Surfaces machined in the first operation, used to locate and dimension the remaining features.

Show which dimensions apply as cast and which after machining, on one drawing or on separate casting and machining drawings. A casting tolerance standard such as ISO 8062 can set general tolerances and machining allowances; agree which standard, if any, applies.

Placeholder for a photo (BH-A16-S06-I01)

Finishes

Machined and as-cast faces often need different finishes, and every finish has to suit the alloy.

Finishes for Cast Aluminum and Zinc

Once trimmed and deburred or blasted, die castings have a smooth surface that suits many coatings. Choose the finish with the alloy, because aluminum and zinc castings take finishes differently.

Powder coating and painting

Common on both alloys for color and corrosion protection. Pretreatment decides adhesion, and porosity near the surface can blister the coating during curing.

Plating

Widely used on zinc die castings for decorative and protective finishes. It shows surface defects clearly, so cosmetic faces need a well-filled casting.

Anodizing

Many aluminum die casting alloys are high in silicon, which makes anodizing uneven and usually gray rather than clear. If a decorative anodized finish is essential, discuss the alloy or consider machining the part.

Mark the faces to be masked, such as machined bores, threads and contact faces, and say whether dimensions apply before or after finishing.

Design Review

With walls, features, machining and finish planned, the design is ready for review before the die is designed.

Ask for a Design Review Before Tooling Starts

A design review checks the part against the way the die will be built and run. Ask for it before the die design is released, while its findings are still edits to the model rather than changes to hardened steel.

A typical review looks at the parting line, gate and ejector positions, slides, porosity-prone sections, and the machining allowance and datums. Record each accepted change in a new revision, and send:

  • The 3D model and drawing, with a clear revision.
  • The alloy, or the properties the part must provide.
  • Machined features, critical dimensions and their datums.
  • Cosmetic faces, sealing requirements and the finish.
  • The first-order quantity and expected repeat demand.

Bohui produces CNC machined, sheet metal, injection molded, 3D printed and vacuum cast parts in its own factory, and also offers aluminum and zinc alloy die casting. Send your design and these details with your quote request.

Discuss the Requirement with Bohui

Share the part information and the decision you need to make.

Placeholder for a contact photo of Jane

Jane

BOHUI PROTOTYPES LIMITED

I'm Jane, the contact for your enquiry.

You can also reach me by email or on WhatsApp.

Jane

BOHUI PROTOTYPES LIMITED

  • Address: Xiaobian Street, Chang'an Town, Dongguan City, Guangdong Province, China

Request a Quote

Fields marked  are required.

Jane BOHUI PROTOTYPES LIMITED Privacy Policy